SQ Cutters

Phone: 330-487-0600

1780 Enterprise Parkway 

​twinsburg, Ohio  44087 


         Common Solutions to Bad Dressings

    Semtorq, Inc.        
       Serving the industry since 1957 with process Automation and Engineering

Our special design cutters will provide you solutions to your dressing problems

     -Optimized cutter designs enable consistent removal

     -Cutters utilize a four blade configuration for balanced                    dressing

     -Semtorq's SQ cutters maximizes cap life


Problem: Electrode is cut but not cleaned at the weld face after first dress

Probable Cause:  -Too high of weld count before first dress

                                 -Too low of dress force

                                 -Not enough dwell time

                                 -check water flow

                                 -Excess heat accelerates mushrooming